| Brand type: | ÕÍ57ÊÂÞÒÌÁË-ÂÈ - ÒÓ 14-1-3780-84 |
|---|---|
| Range | Rod, wire, ring, forging, shaft, sheet, strip, band, tape, pipe, offsets and flanges, various wares of industrial use on demand of a customer |
| Machining | Lathe machining, Milling, Grinding, Deep drilling: max length 9.8 m. |
| Heat treatment | Normalization, annealing, tempering, quenching, quench and temper, holding, shell hardening, carburizing |
| Al | As | B | Bi | C | Ca | Ce |
|---|---|---|---|---|---|---|
| 2.6 - 3.3 | 0.0005 | 0.02 | < 0.00005 | 0.06 - 0.12 | – | 0.015 |
| Co | Cr | Cs | Cu | Fe | Hf | La |
| 10.0 - 11.5 | 15.0 - 16.2 | – | < 0.1 | < 0.5 | 0.8 - 1.4 | – |
| Mg | Mn | Mo | N | Nb | Nd | Ni |
| – | < 0.3 | 1.6 - 2.3 | < 0.01 | 0.1 - 0.3 | – | Îñòàëüíîå |
| O | P | Pb | Re | S | Sb | Sc |
| < 0.008 | < 0.008 | < 0.001 | – | < 0.008 | < 0.0005 | – |
| Si | Ti | Tl | V | W | Y | Zr |
| < 0.3 | 4.0 - 4.8 | – | – | 4.7 - 5.9 | 0.03 | 0.05 |
| Dimension | Value | Measuring units |
|---|---|---|
| Thermal expansion | 10,1 - 17.,1 | Å-6 / K |
| Thermal conducitivity | 55,4 - 75,5 | W / m*K |
| Specific heat | 456 | J/kg*K |
| Melting point | 1370 - 1400 | ° C |
| Working temperature | 0 - 500 | ° C |
| Density | 8000 - 8000 | kg/m3 |